Thermally stable and processible norbornene copolymers Abstract Processible norbornene copolymers were realized by judiciously designing norbornene comonomers, which were themselves prepared by the Diels-Alder reaction of cyclopentadiene and benzoquinone followed by the isomerization and alkylation of alcohols. The norbornene copolymers containing these derivatized comonomers, prepared by [Pd(NCCH2CH3)4][SbF6]2 catalyst, exhibited excellent solubility in many organic solvents as well as good thermal stability, as evidenced by their high glass transition (T g ) and decomposition (∼350°C) temperatures. In addition, fairly strong adhesion to substrates such as glasses and silicon wafers was also achieved with these copolymers to overcome the limitations experienced by polynorbornene homopolymers and to make them attractive for many important industrial applications. http://www.deepdyve.com/assets/images/DeepDyve-Logo-lg.png "Macromolecular Research" Springer Journals

Thermally stable and processible norbornene copolymers

Loading next page...
 
/lp/springer-journals/thermally-stable-and-processible-norbornene-copolymers-xvaKVSxFUZ

References (18)

Publisher
Springer Journals
Copyright
2006 The Polymer Society of Korea and Springer
ISSN
1598-5032
eISSN
2092-7673
DOI
10.1007/BF03219076
Publisher site
See Article on Publisher Site

Abstract

Abstract Processible norbornene copolymers were realized by judiciously designing norbornene comonomers, which were themselves prepared by the Diels-Alder reaction of cyclopentadiene and benzoquinone followed by the isomerization and alkylation of alcohols. The norbornene copolymers containing these derivatized comonomers, prepared by [Pd(NCCH2CH3)4][SbF6]2 catalyst, exhibited excellent solubility in many organic solvents as well as good thermal stability, as evidenced by their high glass transition (T g ) and decomposition (∼350°C) temperatures. In addition, fairly strong adhesion to substrates such as glasses and silicon wafers was also achieved with these copolymers to overcome the limitations experienced by polynorbornene homopolymers and to make them attractive for many important industrial applications.