Get 20M+ Full-Text Papers For Less Than $1.50/day. Start a 14-Day Trial for You or Your Team.

Learn More →

Tensile Damage Mechanism of 3-D Angle-Interlock Woven Composite using Acoustic Emission Events Monitoring

Tensile Damage Mechanism of 3-D Angle-Interlock Woven Composite using Acoustic Emission Events... AbstractThe quasi-static tensile damage behavior of one type of layer-to-layer 3-Dimensional Angle-interlock Woven Composite (3DAWC) was tested and analyzed in this paper. Incorporated with the acoustic emission (AE) events monitoring, the mechanical behavior of the 3DAWC under tensile loading condition was characterized. The Load-Extension curve, Load/AE events-Time curves occurred during the entire testing process and tensile damage modes were recorded to characterize and summarize the mechanical properties and damage mechanism of the 3DAWC subjected to tensile loading. It was found that the tensile damage of the 3DAWC could be summarized into 3 steps. And each step has a distinct primary damage mode. Moreover, the resin cracks, resin-yarn interface debonding and yarn breakages were the main damage modes for the 3DAWC. http://www.deepdyve.com/assets/images/DeepDyve-Logo-lg.png Autex Research Journal de Gruyter

Tensile Damage Mechanism of 3-D Angle-Interlock Woven Composite using Acoustic Emission Events Monitoring

Loading next page...
 
/lp/de-gruyter/tensile-damage-mechanism-of-3-d-angle-interlock-woven-composite-using-Qxqg5uQlpD
Publisher
de Gruyter
Copyright
© 2017 Qian Ma et al., published by De Gruyter Open
ISSN
2300-0929
eISSN
2300-0929
DOI
10.1515/aut-2017-0010
Publisher site
See Article on Publisher Site

Abstract

AbstractThe quasi-static tensile damage behavior of one type of layer-to-layer 3-Dimensional Angle-interlock Woven Composite (3DAWC) was tested and analyzed in this paper. Incorporated with the acoustic emission (AE) events monitoring, the mechanical behavior of the 3DAWC under tensile loading condition was characterized. The Load-Extension curve, Load/AE events-Time curves occurred during the entire testing process and tensile damage modes were recorded to characterize and summarize the mechanical properties and damage mechanism of the 3DAWC subjected to tensile loading. It was found that the tensile damage of the 3DAWC could be summarized into 3 steps. And each step has a distinct primary damage mode. Moreover, the resin cracks, resin-yarn interface debonding and yarn breakages were the main damage modes for the 3DAWC.